Differential scanning calorimetry study of the reactivity of carbon anodes in plastic Li-ion batteries

A. Du Pasquier, F. Disma, T. Bowmer, A. S. Gozdz, G. Amatucci, J. M. Tarascon

Research output: Contribution to journalArticlepeer-review

325 Scopus citations

Fingerprint

Dive into the research topics of 'Differential scanning calorimetry study of the reactivity of carbon anodes in plastic Li-ion batteries'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds